Low-Defect Graphite Oxide
₹ 27000 – ₹ 36000 exc. gst
Low-Defect Graphite Oxide
YAAVIK MATERIALS AND ACS MATERIALS PRESENTS Low-Defect Graphite Oxide in India.
Product Detail
When it comes to utilizing graphite oxide, you need to ensure the compound is stable and guaranteed to remain strong over time. Low-defect graphite oxide that is created through an HI chemical reduction and high-temperature thermal reduction method is proven to be of the highest quality. Whether you plan on using the graphite oxide to manufacture graphene or are aiming to strengthen your water purification technologies, this product is designed to be highly flexible yet immensely strong. This ensures that no matter what the application field is, you’re bound to see quality results after implementing low-defect graphite oxide. For more information on our low-defect graphite oxide, contact us.
CAS-No.: 7782-42-5
1. Preparation Method
HI Chemical Reduction and High-Temperature Thermal Reduction
2. Characterizations
Appearance:
|
Brownish Grey Powder
|
Lateral size:
|
0.5-20 μm
|
pH (1mg/mL):
|
~2.73
|
Singer layer Ratio:
|
>95%
|
Carbon Content:
|
~44.5 wt.%
|
Oxygen Content:
|
~48.9 wt.%
|
Sulfur Content:
|
<1.5 wt.%
|
Ash Content
|
<1.0 wt.%
|
Tap Density:
|
~0.27 g/mL
|
Grain Size:
|
<80 mesh
|
Typical SEM Image of Low-Defect Graphite Oxide
Typical TEM Image of Low-Defect Graphite Oxide
To check out the list of all products visit on https://yaavikmaterials.com/nanoparticles-2/
To visit homepage click on https://yaavikmaterials.com/
Reviews
There are no reviews yet.