High Surface Area Graphene Oxide

 28000 33000 exc. gst

High Surface Area Graphene Oxide

YAAVIK MATERIALS AND ENGG PVT LTD , INDIAN DISTRIBUTOR OF ACS MATERIALS  SUPPLIES BEST QUALITY OF High Surface Area Graphene Oxide IN INDIA.

CAS No.: 7782-42-5

1. Preparation Method:  Modified HUMMER’S method 

2. Characterizations

Type:

Type A

Type B

Appearance:

Brownish Yellow Powder

Brownish Grey Powder

Purity:

~ 99%

~ 99%

Lateral size:

1-5 μm

0.2-10 μm

Thickness:

0.8-1.2 nm

~1 nm

Monolayer Rate:

~ 99%

>90%

Carbon Content:

~51.26 wt.%

~46 wt.%

Oxygen Content:

~40.78 wt.%

~50 wt.%

Sulfur Content:

N/A

<1.5 wt.%

BET:

>100 m2/g

~400 m2/g

* Type A: NEW SKU#: GNOP1101 / OLD SKU#: GnOP1LHS-0.5g

To check out the list of all products visit on https://yaavikmaterials.com/nanoparticles-2/

To visit homepage click on https://yaavikmaterials.com/

Clear
SKU: GNOP11A5 Category: Tag:

Description

YAAVIK MATERIALS AND ACS MATERIALS PRESENTS High Surface Area Graphene Oxide in India. The material synthesized in fully controlled environment and with proven parameters gives you the best desired results. For more information and customized requirements contact info@yaavikmaterials .com

High Surface Area Graphene Oxide

TEM IMAGE

AFM IMAGE

The product is also available on https://www.yaavikmaterials.org/  , https://yaavikmaterials.in/

Attentions

This graphene oxide with high surface area is easier to be oxidized than the normal graphene oxide‚ and it should be kept out of the sun.

*The research demonstrates that a common contaminant (some potassium salt residues) in graphite oxide renders the material highly flammable. The properties of graphene oxide are similar with graphite oxide. ACS Material-Graphene oxide has been purified for many times‚ and the potassium salt is removed completely. Therefore the consumers can use ACS Material-Graphene oxide without any hesitation.
*Kim F‚ Luo J‚ Cruz-Silva R et al. Self-propagating domino-like reactions in oxidized graphite‚ Advanced Functional Materials‚ 2010‚ 20 (17): 2867-2873.

FAQ

How do I disperse single layer Graphene Oxide into a suitable carrier?

For dispersion in water
1) Use distilled or deionized water
2) Add graphene powder
3) Use sonication power of 200W for about 2 hours

For dispersion in ethanol
1) Use pure ethanol
2) Add graphene powder
3) Use sonication power of 200W for about 4 hours

Is Graphene Oxide fully oxidized? What is the C:O ratio?

Graphene Oxide (GO) is produced by the classic modified Hummer’s method‚ which yields an oxidization level of ≥95%.  Regarding the C:O ratio‚ there is some variance inherent in the manufacturing process but the figures below give you an approximation of what to expect:

Sample                 N (wt %)        C (wt %)      O (wt %)     C/O at. ratio
Graphene Oxide          0                51.26           40.78             1.67

NOTE: This graphene oxide with high surface area is easier to be oxidized than the normal graphene oxide‚ and it should be kept out of the sun.

Additional information

Type

Type A, Type B

Packaging

500 mg

Reviews

There are no reviews yet.

Be the first to review “High Surface Area Graphene Oxide”

Your email address will not be published. Required fields are marked *

Product Enquiry